Table 1. Optimized Parameter for Electrospinning F-Gelatin-Based Fibers.
| scaffold type | f-gel | f-gelatin and PCL (1:1) | coaxial f-gelatin > PCL |
|---|---|---|---|
| concentration of polymer(s) | 10% w/v (f-gel) | 5% w/v (f-gel) | 5% w/v (f-gel) |
| 5% w/v (PCL) | 5% w/v (PCL) | ||
| solvent | HFP | HFP | HFP |
| flow rate | 0.5 mL/h | 1 mL/h | core-0.5 mL/h |
| sheath-0.5 mL/h | |||
| accelerating voltage | 1.5 kV/cm | 1.5 kV/cm | 1.5 kV/cm |
| distance between tip and collector | 10 cm | 10 cm | 10 cm |
| average fiber diameter (nm) | 760 ± 80 nm | 420 ± 110 nm | 810 ± 60 nm |