Table 1. DSC Data of n-Octadecane and TSO Compositesa.
cooling |
heating |
||||||||
---|---|---|---|---|---|---|---|---|---|
sample | ω (%) | Tc (°C) | Toc (°C) | ΔHc (J/g) | Tm (°C) | Tom (°C) | ΔHm (J/g) | ΔHm* (J/g) | η (%) |
n-octadecane | 24.25 | 25.17 | 227.93 | 29.37 | 25.85 | 228.21 | |||
TSO-1 | 62.32 | 22.32 | 24.20 | 137.52 | 29.04 | 24.93 | 137.99 | 142.22 | 97.03 |
TSO-2 | 58.75 | 22.89 | 23.91 | 129.81 | 29.05 | 24.71 | 130.35 | 134.08 | 97.22 |
TSO-3 | 54.40 | 23.11 | 23.64 | 119.95 | 28.30 | 24.51 | 120.65 | 124.14 | 97.19 |
TSO-4 | 48.94 | 21.74 | 23.36 | 108.03 | 28.29 | 24.30 | 108.78 | 111.70 | 97.39 |
Note: ΔHm* = .