Magnetic parameters for MnxZn1−xCo2O4 samples measured at temperatures of 300 K and 10 K.
| Sample | 300 K | 10 K | ||||
|---|---|---|---|---|---|---|
| M s (emu g−1) | M r (emu g−1) | H c (kOe) | M s (emu g−1) | M r (emu g−1) | H c (kOe) | |
| ZnCo2O4 | 0.01 | 0 | 0 | 1.82 | 0 | 0 |
| Mn0.3Zn0.7Co2O4 | 0.4 | 0 | 0 | 3.15 | 0.07 | 0.3 |
| Mn0.5Zn0.5Co2O4 | 0.55 | 0 | 0 | 3.51 | 0.25 | 1.32 |
| Mn0.7Zn0.3Co2O4 | 0.87 | 0 | 0 | 5.92 | 1.15 | 1.93 |
| MnCo2O4 | 1.3 | 0.12 | 1.2 | 4.08 | 1.03 | 3.02 |