Synthetic strategies used for each MNP@lignin compositea.

MNP@lignin Mass ratio (mg of metal precursor/mg of lignin) Irradiation T (°C) t (min)
AuNP@alkali 0.5 532 nm 25 5
AuNP@ZHL 1 Dark 58 10
AuNP@AL 2 Dark 58 30
AgNP@alkali 5 465 nm 28 5
AgNP@ZHL 1 Dark 58 5
AgNP@AL 1 465 nm 28 5
a

Conditions: 0.1 mg of lignin in water or pH 12 according to lignin solubility.