TGA of Av and Av-cl-poly(AA-ipn-AAm).

Sample Code Thermogravimetric analysis
First stage decomposition (°C), pyrolysis weight loss of polymer content (%) Second stage decomposition (°C), pyrolysis weight loss of polymer content (%) Third stage decomposition (°C), pyrolysis weight loss of polymer content (%)
Av 110 °C, 24.4% 110–205 °C, 46.2% 205–280 °C, 28.9%
IPN 110 °C, 23.4% 110–205 °C, 22.4% 205–280 °C, 28.9%