TABLE 2.
Sample | Thickness (mm) | Tensile strength (MPa) | Youngs modulus (MPa) | Elongation at break(%) |
---|---|---|---|---|
Control | 0.21 ± 0.02 | 2.75 ± 0.3 | 25.22 ± 1.2 | 10.4 ± 1.2 |
10 NE | 0.22 ± 0.01 | 3.45 ± 0.2 | 28.55 ± 1 | 11.2 ± 0.96 |
25 NE | 0.23 ± 0.02 | 3. 52 ± 0.3 | 29.14 ± 0.7 | 15 ± 0.3 |
50NE | 0.22 ± 0.02 | 3.50 ± 0.18 | 28.27 ± 1.24 | 13.2 ± 1.44 |