Results of Cochran’s Q test for the roughness parameters on the end face of the AZ91D magnesium alloy, λs = 20° tool.

λs = 20° End Face of the AZ91D
Cochran’s Q Test
Roughness Parameter vc 400 vs. 1200 fz 0.05 vs. 0.3
Mean Mean Test * df p-Value Mean Mean Test * df p-Value
Ra 2.3714 1.3818 3.4085 4.100354 0.026035 0.8712 1.786 -5.9069 4.583435 0.00265
Rz 13.128 6.412 4.3650 4.022686 0.011865 4.166 7.97 -4.6056 4.361437 0.008121
RSm 0.1196 0.1716 −1.0226 4.590582 0.357305 0.1014 0.2248 -3.6712 4.409552 0.018011
Rsk 0.334 −0.3034 3.5067 4.432405 0.020918 0.05 0.2152 -0.7847 4.105744 0.475401
Rku 2.9146 2.2392 1.6676 4.217333 0.167024 - - - - -