The enhancement of the MG adsorption yield and capacity on the Fe3O4 NP surfaces by thermocatalysis.
Sample | 298.15 K | 303.15 K | 308.15 K | 313.15 K | 318.15 K | |||||
---|---|---|---|---|---|---|---|---|---|---|
q eI (mg g−1) | R I% | q eII (mg g−1) | R II% | q eII(mg g−1) | R II% | q eII(mg g−1) | R II% | q eII (mg g−1) | R II% | |
MG/ARM-Fe3O4 | 15.81 | 53.42 | 17.01 | 57.48 | 18.00 | 60.81 | 18.53 | 62.61 | 18.98 | 65.01 |
MG/ROS-Fe3O4 | 15.37 | 51.90 | 16.32 | 55.64 | 16.75 | 57.09 | 17.81 | 60.83 | 18.80 | 64.09 |
MG/MAT-Fe3O4 | 10.83 | 35.91 | 12.69 | 42.88 | 14.53 | 49.10 | 17.01 | 57.48 | 18.56 | 63.60 |
MG/JUN-Fe3O4 | 05.70 | 19.25 | 06.59 | 22.25 | 07.87 | 26.58 | 11.49 | 38.83 | 13.49 | 45.59 |