Light microscopic images of the HEBM composite powders produced by (a) Reference, (b) Program1 (Speed), (c) Porgram2 (Menthol), and (d) Porgram3 (Argon) after a thermal post-treatment in a tube furnace (TF) at 515 °C for 3.5 h.