Skip to main content
. 2022 Apr 23;14(9):1729. doi: 10.3390/polym14091729

Figure 8.

Figure 8

(a) SEM micrograph of the AAF (top)—expanded clay (bottom) interface, element maps of an EDXS scan performed on the framed area are presented below. (b) The same, but at a different location.