. 2022 Apr 28;14(9):1799. doi: 10.3390/polym14091799

Figure 8.

Figure 8

SEM images of fracture surfaces of fibre-reinforced AA mortars after accelerated carbonation for: (a) fly-ash-based AA mortar (FA1); (b) fly-ash-and-GBFS-based AA mortar (FA2S).