Skip to main content
. 2022 Apr 23;15(9):3076. doi: 10.3390/ma15093076

Figure 7.

Figure 7

Fracture surfaces of H13 steel after tensile test for cooling rate of: (a) 100 °C/s; (b) 10 °C/s; (c) 1 °C/s.