Filler Type Filler Percentage (%) Peak Area at Initial Time (cm2) Peak Area after 3D Printing (cm2) Conversion (%)
MCC 0.15 195.23 8.36 95.7
0.30 200.92 7.56 96.2
0.60 200.54 0.17 99.9
1.20 200.73 1.84 99.1
2.40 186.96 7.77 95.8
CNC 0.15 175.08 2.17 98.8
0.30 173.32 5.29 96.9
0.60 177.20 1.08 99.4
1.20 173.34 7.78 95.5
2.40 187.90 7.12 96.2