Skip to main content
. 2022 Apr 28;14(9):1810. doi: 10.3390/polym14091810

Figure 2.

Figure 2

Deconvolution of the peaks seen on the scans registered for MC content: (a) 1 wt%, (b) 3 wt%, (c) 9 wt% during heating, and (d) 1 wt% during cooling.