Fig. 3. Mass change in water by solar-to-steam generation for (a) ACLA-C with different loading amounts of AC-C, and (b) ACLA-C_PEI with different concentration of PEI polymer. (c) The cyclic test with drying samples after each measurement using ACLA-C (20 mg mL−1). (d) The time-on-stream evaporation rate of salt water by ACLA-C (20 mg mL−1). All the measurements are performed under the irradiance of 1 sun for 1 h.