Skip to main content
. 2022 May 6;7(19):16778–16784. doi: 10.1021/acsomega.2c01675

Figure 2.

Figure 2

XRD patterns for p(DDA/TMSPA1) (top), p(DDA/TMSPA13) (center), and p(DDA/TMSPA32) (bottom) thin films annealed at 80 °C for 1 h under vacuum.