Properties of different samples.

Sample Viscosity of Electrospun Solution (mPa.S) Average Fiber Diameter (nm) Porosity
(%)
SF 438 ± 2 376 ± 7 49.9 ± 1.20
SF-GP 470 ± 9 390 ± 5 40.5 ± 3.01
SF-CG1-GP 533 ± 2 410 ± 2 53.2 ± 4.21
SF-CG3-GP 580 ± 7 450 ± 3 57.5 ± 5.1
SF-CG5-GP 617 ± 2 501 ± 6 61.5 ± 3.3