Mechanical characterization of MASO3 (2 mol/L) with BAP (2 mol%) as a crosslinker: (a) technical stress-strain curves of three single measurements with the swollen hydrogel until breakage and (b) linear interpolation of the data from ɛ = 2−7% to determine the compressive modulus.