Skip to main content
. 2022 May 12;15(10):3476. doi: 10.3390/ma15103476

Figure 8.

Figure 8

Efficiency factors of ceramic fillers on CTE reduction versus ceramic volume fractions. Efficiency factors of fused silica fillers within Alumix-231 matrix, sintered at 565 °C, were plotted. Efficiency factors for ZrMgMo3O12, SiC, Al2O3 and Si3N4 are available from literature [36,39,40,41].