Skip to main content
. 2022 May 19;14(10):2079. doi: 10.3390/polym14102079

Figure 7.

Figure 7

Damage on the composite panels seen after the quasistatic indentation test. The specimen dimensions are 100 mm × 100 mm × 20 mm.