Skip to main content
. 2022 May 13;14(10):1986. doi: 10.3390/polym14101986

Figure 1.

Figure 1

(a,b) The digital photo images of the 98 wt% CoSb2.95Te0.05/PEDOT:PSS hybrid film; SEM images of (c) pristine PEDOT:PSS-5% DMSO, (d) 20 wt%, (e) 40 wt%, (f) 60 wt%, (g) 80 wt%, (h) 90 wt% and (i) 98 wt% CoSb2.95Te0.05 hybrid film; (j) the corresponding EDX mapping images of Co, Sb, Te, C, O, and S; and (k) cross-sectional SEM image of the 98 wt% CoSb2.95Te0.05 hybrid film.