Skip to main content
. 2022 May 10;15(10):3425. doi: 10.3390/ma15103425

Figure 14.

Figure 14

SEM images of sample Al-2-1 corroded by slag S (1350 °C, 10 h); (a,c) hot-face zone of the impregnated area, (b,d) high magnification of ho-face zone (slag/refractory interface).