Figure 8.

Figure 8

Graph of maximum wall shear stress at varying inlet pressure for bioinks with different power-law constant using (A) tapered conical nozzle (Dout = 0.3 mm), (B) conical nozzle (Dout = 0.3 mm), and (C) cylindrical nozzle (Dout = 0.3 mm).