Skip to main content
. 2022 May 25;15:100295. doi: 10.1016/j.mtbio.2022.100295

Table 2.

Surface element percentages and stiffness of the SP scaffold before and after PDA coating.

Atomic concentration (%) C 1s O 1s N 1s Stiffness (MPa)
Before 79.3 20.7 0 141.4 ​± ​9.2
After 76.1 17.0 6.9 121.0 ​± ​1.8