Skip to main content
. 2022 May 20;8(6):e09442. doi: 10.1016/j.heliyon.2022.e09442

Table 4.

Tan δ and E′ of hybrid BC/Kevlar composites.

Sample Tg from Tan δ (°C) Tan δ Storage Modulus (E′) (MPa) Storage modulus percentage performance of composite compared to K/K/K composite (%)
K/K/K 63.73 0.271 408 -
K/BC/K 69.90 0.235 639 +56
BC/K/BC/K/BC 70.26 0.223 1120 +174
K/3BC/K 56.78 0.295 348 -17
2BC/K/2BC/K/2BC 59.49 0.344 381 -6
3BC/2K/3BC 65.97 0.298 630 +54
K/6BC/K 50.39 0.254 205 -49