Skip to main content
. 2022 Jun 7;12(26):16875–16885. doi: 10.1039/d2ra01459a

Weight fraction of t-ZrO2 (ωt-ZrO2) and mean crystallite size (dc) for zirconia samples calcined at 973 K with different mole fractions of Si (yS). Values and error ranges calculated from Rietveld refinement. For detailed information, see Section S3.1 in the ESI.

Sample ω t-ZrO2/wt% d c/nm
Pure ZrO2 4.72(16) 23.7(6)
5SZ 78.6(2) 15.4(2)
8SZ 98.84(15) 13.9(2)
15SZ 100 13.4(5)
19SZ 100 7.5(3)
27SZ n.a.a n.a.a
a

Not applicable.