Fig. 3. Electron micrology studies on RuNi catalysts.

Fig. 3

a HAADF–STEM image, b corresponding EDS mapping images, c high-resolution AC–HAADF–STEM image, and d enlarged STEM image and corresponding intensity profile of 0.4 wt.% RuNi sample. e, f AC–HAADF–STEM images of the 0.6 wt.% RuNi and 2 wt.% RuNi samples, respectively.