Skip to main content
. 2022 May 30;14(11):2218. doi: 10.3390/polym14112218

Figure 15.

Figure 15

The comparison of temperatures (a) at measuring points with different inlet temperatures and comparison of simulation and experiment with the inlet temperature of (b) 200 °C, (c) 300 °C, and (d) 400 °C with a heating time of 20 s and stamp thickness of 1.1 mm.