Comparison of XRD patterns of the original and additionally heat-treated sensors (Inline graphic: Al2O3, Inline graphic: Pt, Inline graphic: ZnO peak, (a,c) U30 sensor; (b) U30-N sensor; (d) U30-O sensor).