. 2022 Jun 15;12:9955. doi: 10.1038/s41598-022-13705-0

Figure 3.

Figure 3

XRD patterns (a) 2θ = 27.5°–32.5°, (b) 2θ = 72.5°–75.5°, and (c) Raman spectra of 8.5YSZ ceramics after heat treatment for different times.