Table 1.
One-way ANOVA test result for enamel surface damage from three groups
| Post-debond enamel loss measured on OCT in µm | plier | Ultrasonic scaler | Laser |
|---|---|---|---|
| N | 10 | 23 | 12 |
| Mean | 31.1 | 55.7 | 33.7 |
| SD | 6.3 | 10.0 | 6.0 |
| Minimum | 22.0 | 42.0 | 24.0 |
| Maximum | 42.0 | 84.0 | 42.0 |
| First quartile | 25.5 | 48.0 | 28.5 |
| Median | 31.0 | 54.0 | 33.0 |
| Third quartile | 36.5 | 58.0 | 39.5 |
F=43.523 P<0.001