Composition of pure iron used for manufacturing SLM, LMD and casting in wt.% (Reprinted with permission from Ref. [26]. Copyright @ 2019, Wiley Online Library).

Sample Density ρ (g/cm³) Young’s Modulus (GPa) Compressive Strength at 20% Strain (MPa)
SLM 7.87 199.7 ± 6.7 760.2 ± 6.5
LMD 7.84 202.5 ± 5.3 580.6 ± 4.2
Cast 7.81 202.5 ± 6.7 497.8 ± 7.5