The failure rate of restorative materials at 36 months. Abbreviations: A: amalgam; CO: compomer; GIC: glass-ionomer cement; HVGIC: high-viscosity glass-ionomer cement; MRGIC: metal-reinforced glass-ionomer cement; RC: resin composite; RMGIC: resin-modified glass-ionomer cement; SSC: stainless steel crown; n: represents the number of reviews in which the efficacy of the specific material was assessed; Min: minimum value for failure rate; Max: maximum value for failure rate.