Table 2.
Viscosity and Conductivity of the electrospinning precursor fluid.
| Samples | PAN | M. bontioides | Ag | Ag-CN | Viscosity/(mPa s) | Conductivity/(ms cm−1) |
|---|---|---|---|---|---|---|
| PAN | 8 wt% | / | / | / | 1650 ± 0.82 | 0.0891 ± 0.0037 |
| PAN/M. bontioides | 8 wt% | 5 wt% | / | / | 266 ± 1.63 | 0.1023 ± 0.0005 |
| PAN/M. bontioides /Ag | 8 wt% | 5 wt% | 5 wt% | / | 340.33 ± 2.87 | 1.7537 ± 0.0021 |
| PAN/M. bontioides/Ag-CN/Ag | 8 wt% | 5 wt% | 5 wt% | 1 wt% | 405.67 ± 2.87 | 2.4267 ± 0.0170 |