Figure 1.

Figure 1

Digital photos of samples at room temperature (25 °C), at or above gelling temperature (T > LCST), and at room temperature (25 °C) (In the example, the thermosensitive gel was composed of poloxamer 407, poloxamer 188, and carbomer).