Skip to main content
. 2022 Jun 7;14(24):28211–28220. doi: 10.1021/acsami.2c05218

Table 2. Growth Parameters for the Four Pd Electrical Contacts Here Studied Together With the Resistance and Resistivity Values for Each Pt Nanowire.

sample spin-coated initial thickness [nm]a Ga+ dose for Pd microstructures [μC/cm2] resistance [kΩ] resistivity [103 μΩ·cm]b
NW_Pt-FIBID_1 350 30 235 9.2
NW_Pt-FIBID_2 200 30 247 9.2
NW_Pt-FIBID_3 125 30 147 5.4
NW_Pt-FIBID_4 125 10 189 7.0
a

Value corresponding to the initial thickness of the spin-coated film before the Ga+ irradiation.

b

Value calculated considering that all nanowires have a width of 100 nm and a thickness of 30 nm.