Figure 2.

Figure 2

Storage modulus as a function of frequency for PP-based composites containing BC particles obtained at: (a) 700 °C and (b) 900 °C [52]. Reproduced with permission from Elsevier Science Ltd. 2018, Elsevier Science Ltd.