Skip to main content
. 2022 Jun 11;14(6):1238. doi: 10.3390/pharmaceutics14061238

Table 3.

Effect of chitosan hydrochloride or carboxymethyl chitosan addition on particle size, zeta-potential, and poly dispersity index (PDI) of hybrid NPs formulated by the w/o/w double emulsion method (mean ± SD, n = 3).

Chitosan Hydrochloride (1 mg/mL) Carboxymethyl Chitosan *
Size (nm) Charge (mV) PDI Size (nm) Charge (mV) PDI
PGA-co-PDL 291.0 ± 9.2 17.4 ± 1.0 0.09 ± 0.04 280.5 ± 8.8 −20.1 ± 1.5 0.13 ± 0.02
PLGA 310.2 ± 6.0 13.2 ± 0.8 0.10 ± 0.03 299.4 ± 7.1 −40.5 ± 0.9 0.09 ± 0.07

* Carboxymethyl chitosan 1 mg/mL for PGA-co-PDL formulation and 0.5 mg/mL for PLGA formulation.