. 2022 Jun 7;12(12):1956. doi: 10.3390/nano12121956

Figure 4.

Figure 4

Cross-sectional TEM images of SiOx blending electrode after (a) 50 cycles, (b) 100 cycles, and (c) 250 cycles.