Figure 1.

Figure 1

XRD spectra of Sr-TCP, Mg-TCP, and β-TCP control samples sintered at 1250 °C. The α-TCP peak at 30.7° visible in β-TCP and Sr-TCP is not present in Mg-TCP. β-TCP and α-TCP peaks identified according to ICDD 09-0169 and 09-0348, respectively.