Skip to main content
. 2022 Jun 29;13:3754. doi: 10.1038/s41467-022-31427-9

Fig. 2. Phase and coordination environment for dCu2O/Ag catalysts.

Fig. 2

a HAADF–STEM image with EDS elemental mappings and b high resolution STEM image of dCu2O/Ag2.3%. c Enlarged XRD patterns for dCu2O, dCu2O/Ag2.3% and dCu2O/Au2.3%. d In situ XANES spectra and e Wavelet transform images of EXAFS data with optimized Morlet parameter (i.e., κ = 5, σ = 1) at Cu K-edge for commercial Cu-foil, dCu2O, dCu2O/Ag2.3% and dCu2O/Au2.3%. Fourier transform curves of in situ EXAFS data and corresponding fitted results (first coordination shell) for f dCu2O, g dCu2O/Ag2.3% and h dCu2O/Au2.3%. Scale bars, 10 nm in (a) and 1 nm in (b).