Table 2. Electrochemical Parameters of the Uncoated and Coated Matrix.
| coatings | Ecorr [V] | Icorr [A/cm2] | CR [mm/a] | PE [%] |
|---|---|---|---|---|
| blank | –0.508 | 6.37 × 10–6 | 1.48 × 10–1 | |
| epoxy resin coating | –0.472 | 2.97 × 10–7 | 6.91 × 10–3 | 95.65 |
| self-healing coating | –0.303 | 8.32 × 10–9 | 1.94 × 10–4 | 99.87 |