Skip to main content
. 2020 Dec 28;1(1):69–81. doi: 10.3877/cma.j.issn.2096-112X.2020.01.007

Table 2. Range analysis of compression strength and porosity of hydroxyapatite/aragonite.

Factors Pressure (MPa) Printing speed (mm/s) Distance between strands (mm)
Compression strength
 k1 2.01 1.55 1.54
 k2 1.35 1.44 1.44
 k3 0.78 1.15 1.16
 R 1.23 0.4 0.38
Porosity
 k1 39.1 40.0 39.3
 k2 27.3 36.0 38.0
 k3 39.2 39.7 38.3
 R 11.9 3.0 1.0