. 2022 Jun 28;15(13):4535. doi: 10.3390/ma15134535

Table 3.

Thickness and roughness of MAO coatings before (bT) and after (aT) TCT.

Sample
Code
Thickness, μm Roughness, μm
Ra Rz
Ti-without MAO 5.6 32.1
Ti-MAO-10-30_bT 27.2 2.3 14.9
Ti-MAO-10-60_bT 42.6 3.7 22.0
Ti-MAO-20-30_bT 42.8 4.3 25.3
Ti-MAO-20-60_bT 66.4 4.9 27.4
Ti-MAO-10-30_aT 15.2 2.2 14.5
Ti-MAO-10-60_aT 36.4 2.7 15.5
Ti-MAO-20-30_aT 38.8 3.3 18.7
Ti-MAO-20-60_aT 61.6 4.3 22.1