Figure 9.

Figure 9

Particle size distribution for hydrogels with 0.7% (w/v) PVA, 20 μg/mL GO-Ag NPs, 1.1% (w/v) gelatin (A) and 1.5% (w/v) gelatin (B) freshly prepared and evaluated at 28 days exposure to accelerated aging conditions at 40 °C and 75% RH.