(a) Voltage (Ecell) and (b) high-frequency resistance (HFR) versus j curves. The catalysts are at the cathode, PtRu/C 0.36 mgPt/cm2, and at the anode, IrO2 0.75 mgIr/cm2. Dilute KOH or deionized (DI) water serves as the liquid electrolyte. Hexamethyltrimethylammonium-functionalized Diels–Alder polyphenylene (HTMA-DAPP) is used as the AEM and AIE. The AEM wet thickness is 50 μm. All the measurements were conducted at 60 °C and ambient pressure. Reprinted with permission from ref (446). Copyright 2021 IOP Publishing.