Figure 3.

Figure 3

(A) Thickness dependence of the polymer membranes with PEO45-b-PEHOx20 and PMOXA10-b-PDMS25 molar fractions for the investigated samples. (B) Contact angle dependence of polymer membranes with PEO45-b-PEHOx20 and PMOXA10-b-PDMS25 molar fractions, measured with water as the probe liquid. For each point, the measurements were performed at least three times for three different membranes.