Skip to main content
. 2021 Nov 2;14(24):5470–5475. doi: 10.1002/cssc.202101518

Figure 3.

Figure 3

Kinetic profile for degradation of a PLLA sample. [PLA]0=0.44 m; [polyester linkages]0/[Zn]0=60; THF‐d8 (0.45 mL) as solvent; MeOH 0.05 mL.