Figure 3.

Figure 3

Fracture topography of RBF-failed specimens: (a,c) the low and high magnification fracture topographies caused by a Ca-Al-O inclusion respectively; (b,d) the lower and higher magnification fracture topographies caused by a TiN inclusion respectively; (e,f) TiN inclusion crack source; (d,e,f) the position indicated by the red arrow indicates that cracks preferentially initiate at the sharp corners of TiN inclusions.