SEM images (AD) of surface roughness at baseline, 24 h, 96 h and 168 h in citrate buffer. (A): Baseline SEM photomicrograph of IPS e.max ceramic before immersion in citrate buffer (×5000). (B): SEM photomicrograph of IPS e.max ceramic after 24 h immersion in citrate buffer (×5000). (C): SEM photomicrograph of IPS e.max ceramic After 96 h immersion in citrate buffer (×5000). (D): SEM photomicrograph of IPS e.max ceramic after 168 h immersion in citrate buffer (×5000).